- NdFeB Magnets
- SmCo Magnets
- Cast Alnico Magnets
- Hard Ferrite Magnets
- Magnetic Lifter
- Permanent Magnets
- Sintered NdFeB Magnets
- Sintered AlNiCo
- Sintered SmCo
- Neodymium Magnets
- Standard permanent magnetic chuck
- Dense permanent magnetic chuck
- Super Electric Permanent magnetic chuck
- Electric Permanent magnetic chuck
- Magnetic Materials
Tel:
0086-574-27903196
Fax:
0086-574-27903199
Add:
no.65 dahetou road,ningbo,china
Email:
info@mademagnet.com
MSN:
jasonchenqj71@hotmail.com
Certificate
Sintered SmCo
Sintered SmCo Magnet (SmCo magnets, magnetic rings, magnetic tiles, block magnets, magnetic cylinder, rare earth magnets, disc magnets,strong magnets, powerful magnets, permanent magnet)
Sintered Samarium Cobalt Magnet ¡®s biggest advantage is its high working temperature---350℃,in general ,magnetizing field of approximately 30 to 45 KOe are required. SmCo magnet is widely used in motors, meters, transducers, instruments, positional detector, generators , wind power generators, radar and other applications.
Process Flow:
Raw material-----Mixing-----Melting-----Power-----Pressing-----Sintering----Magnetic Inspection-----Cutting and Grinding-----Inspection-----Packing and Shipping
MAGNETIC AND PHYSICAL PROPERTIES OF SINTERED SMCO MAGNET
| Grade | SmCo18 | SmCo20 | SmCo22 | SmCo24 | SmCo24 | SmCo26L | |
| Br | Mt | 840 | 890 | 930 | 980 | 980 | 1030 |
| Gs | 8400 | 8900 | 9300 | 9800 | 9800 | 10300 | |
| Hcj | KA/m | 605 | 637 | 637 | 676 | 676 | 398 |
| Oe | 7600 | 8000 | 8000 | 8500 | 8500 | 5000 | |
| Hcb | KA/n | 1432 | 1432 | 1432 | 1432 | 1989 | 438 |
| Oe | 18000 | 18000 | 18000 | 18000 | 25000 | 5500 | |
| (BH)max | KJ/m3 | 143 | 159 | 175 | 191 | 191 | 207 |
| MGOe | 18 | 20 | 22 | 24 | 24 | 26 | |
| Density | g/cm3 | 8.1 | 8.2 | 8.2 | 8.3 | 8.3 | 8.3 |
| Temperature Coefficient | Near Br %/K | -0.04 | -0.04 | -0.04 | -0.03 | -0.03 | -0.03 |
| Near Hcj %/K | -0.3 | -0.3 | -0.3 | -0.2 | -0.2 | -0.2 | |
| Curie Temperature Tc | ℃ | 750 | 750 | 750 | 800 | 800 | 800 |
| Maximum Working Temperature Tw | ℃ | 250 | 250 | 250 | 280 | 280 | 300 |
| Grade | SmCo26 | SmCo26 | SmCo26 | SmCo28 | SmCo28 | SmCo30 | SmCo30 | |
| Br | Mt | 1030 | 1030 | 1030 | 1070 | 1070 | 1100 | 1100 |
| Gs | 10300 | 10300 | 10300 | 10700 | 10700 | 11000 | 11000 | |
| Hcj | KA/m | 716 | 716 | 716 | 756 | 756 | 772 | 772 |
| Oe | 9000 | 9000 | 9000 | 9500 | 9500 | 9700 | 9700 | |
| Hcb | KA/n | 1194 | 1592 | 1989 | 1194 | 1592 | 1194 | 1592 |
| Oe | 15000 | 20000 | 25000 | 15000 | 20000 | 15000 | 20000 | |
| (BH)max | KJ/m3 | 207 | 207 | 207 | 223 | 223 | 239 | 239 |
| MGOe | 26 | 26 | 26 | 28 | 28 | 30 | 30 | |
| Density | g/cm3 | 8.3 | 8.3 | 8.3 | 8.3 | 8.3 | 8.3 | 8.3 |
| Temperature Coefficient | Near Br %/K | -0.03 | -0.03 | -0.03 | -0.03 | -0.03 | -0.03 | -0.03 |
| Near Hcj %/K | -0.2 | -0.2 | -0.2 | -0.2 | -0.2 | -0.2 | -0.2 | |
| Curie Temperature Tc | ℃ | 800 | 800 | 800 | 800 | 800 | 800 | 800 |
| Maximum Working Temperature Tw | ℃ | 300 | 300 | 330 | 300 | 300 | 300 | 300 |